Wholesale Dealers of Iron Alloy Precision Alloy UNS N08031 Alloy 31 to Mauritius Manufacturers
As for competitive prices, we believe that you will be searching far and wide for anything that can beat us. We can state with absolute certainty that for such quality at such prices we are the lowest around for Wholesale Dealers of Iron Alloy Precision Alloy UNS N08031 Alloy 31 to Mauritius Manufacturers, Let's cooperate hand in hand to jointly make a beautiful future. We sincerely welcome you to visit our company or contact us for cooperation!
HY A31 Material grades and equivalents
AISI/ASTM Alloy 31 / UNS N08031 / W.Nr 1.4562
Chemical composition:
| Alloy | % | Ni | Cr | Fe | Mo | N | C | Mn | Si | 硫 | 铜 | 磷 |
| HY A31 | Min | 30 | 26 | 余量 | 6 | 0.15 | 1 | |||||
| Max | 32 | 28 | 7 | 0.25 | 0.015 | 2 | 0.3 | 0.01 | 1.4 | 0.02 | ||
| Physical properties: | ||||||||||||
| Density | 8.1 g/cm3 | |||||||||||
| Melting point | 1350-1370 ℃ | |||||||||||
| Alloy minimum mechanical properties in the room temperature: | ||||||||||||
| Alloy | Tensile strength Rm N/mm² | Yield strength Rp0.2 N/mm² | Elongation A5 % | |||||||||
| Solution | 650 | 350 | 35 | |||||||||
Characteristic as below:
HY A31 is a nitrogen-containing iron-nickel-molybdenum alloy performance between super austenitic stainless steel and nickel-based alloy, suitable for used in chemical and petrochemical, environment engineering, oil and gas production industrial fields.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China