Wholesale Distributors for Iron Alloy Precision Alloy Invar 36 UNS K93600 Wholesale to Jakarta
We insist on offering high quality production with good business concept, honest sales and the best and fast service. it will bring you not only the high quality product and huge profit, but the most significant is to occupy the endless market for Wholesale Distributors for Iron Alloy Precision Alloy Invar 36 UNS K93600 Wholesale to Jakarta, We will wholeheartedly welcome all clients in the industry both at home and abroad to cooperate hand in hand, and create a bright future together.
HY I36 Material grades and equivalents
GB 4J36/UNS K93600/AISI/ASTM Invar36/W.Nr.1.3912/Pernifer 36
Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Co |
Mo |
P |
S |
|
HY I36 |
Min. |
35 |
Balance |
||||||||
|
Max. |
38 |
0.5 |
0.1 |
0.06 |
0.35 |
1.0 |
0.5 |
0.02 |
0.025 |
Physical properties
|
Density |
8.1 g/cm3 |
|
Melting point |
1430 °C |
Mechanical properties in the room temperature
|
Alloy state |
Tensile strength Rm N/mm2 |
Yield strength RP0.2N/mm2 |
Elongation A5 % |
Brinell hardness HB |
|
HY I36 |
490 |
240 |
42 |
≤200 |
Characteristic
HY I36 alloy is a special ultra-low coefficient of heat expansion of low-iron-nickel alloy. One of carbon and manganese element of control is very important. Cold deformation can reduce the coefficient of thermal expansion, in particular within the framework of the heat treatment temperature coefficient of thermal expansion will enable stabilization. Has the following characteristics:
1.Has very low coefficient of heat expansion between the temperature of -250°C and 200°C.
2.Good toughness and plastic
Metallurgical structure
HY I36 is the face centered cubic lattice structure
Corrosion resistance
HY I36 has corrosion resistance in the dry air of room temperature. In other harsh environments, such as the humid air, there may be corrosion (rust).
Applied field
HY I36 suit for need to apply ultra-low coefficient of heat expansion environment. Typical applications are as follows:
1.Liquefied gas production, storage and transport
2.The measurement and control instruments work temperature lower than 200°C, such as temperature regulating device
3.Metals and other materials use the screw connector bush
4.Bimetal and bimetallic temperature controller
5.Film framework
6.Shadow mask
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen Town GuangDong Province China