Our company insists all along the quality policy of "product quality is base of enterprise survival; customer satisfaction is the staring point and ending of an enterprise; persistent improvement is eternal pursuit of staff" and the consistent purpose of "reputation first, customer first" for Wholesale Price Nickel Alloy Monel K500 UNS N05500 for Liverpool Manufacturers, We sincerely welcome overseas customers to consult for the long-term cooperation and the mutual development.


HY MK-500  Material grades and equivalents

Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500


HY MK-500 Chemical composition:

            Alloy

%

Ni

Cu

Al

Ti

Fe

Mn

S

C

Si

Monle K500

Min.

63

27.0

2.30

0.35

Max.

33.0

3.15

0.85

2.0

1.5

0.01

0.25

0.5

HY MK-500 Physical properties:

Density

8.44 g/cm3

Melting point

1315-1350℃

HY MK-500 minimum mechanical properties in the room temperature:

Forms Condition Max. section Thickness,in.(mm) Tensile strength Min. Ksi.(Mpa) Yield strength Min.Ksi.(Mpa) Elongation in 2 in,or 4D,min.,% Hardness
HB min. HRC min.
Round bars, Hexagons, squares, rectangles and forgings hot-worked and age hardened All Sizes 140(965) 100(690) 20 265 27
Round bars cold worked and age hardened 1/4(6.4)to 1(25.4) 145(1000) 110(760) 15 300 32
over 1(25.4)to 3(76.2) 140(965) 100(690) 17 280 29
over 3(76.2)to 4(101.6) 135(930) 99(655) 20 255 25
Hexagons cold worked and age hardened 1/4(6.4)to 2(50.8) 140(965) 100(690) 15 265 27
Round bars, Hexagons, squares, rectangles and forgings Annealed and age hardened Up to 1(25.4) 130(895) 90(620) 20 250 24
1(25.4)and over 130(895) 85(585) 20 250 24

HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.

Industries Served:

  • gas & oil extraction
  • chemical processing
  • marine engineering
    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !