Cemented carbide YG6X-1
YG6X-1 Material grades and equivalents
|
Trademark |
UNS |
ISO |
AISI/ASTM |
|
YG6X-1 |
K20 |
Chemical composition(mass fraction)(%)
|
Alloy
|
WC |
TiC |
TaC (NbC) |
Co |
Other |
|
YG6X-1 |
- |
Physical properties &minimum mechanical properties
|
Density/ g/cm |
Min Hardness/HRA |
Tensile strength/MPa |
Impact toughness j/cm |
Min Bending strength/ N/cm2 |
|
|
14.6-15.0 |
- |
1500 |
YG6X-1 Processing conditions and application:
It is suitable for cast iron, non-ferrous metals and their alloys of the essence in continuous cutting non-metallic materials, continuous cutting of semi finished car, fine cars, small cars, coarse thread, in the cross section of the continuous half essence milling and milling, rough wisdom and essence of expanding hole.