13 Years Factory wholesale Nickel Alloy Nimonic 80A UNS N07080 to Manchester Factories
owing to good service, a variety of high quality products, competitive prices and efficient delivery, we enjoy a good reputation among our customers. We are an energetic company with wide market for 13 Years Factory wholesale Nickel Alloy Nimonic 80A UNS N07080 to Manchester Factories, We are confident to make great achievements in the future. We are looking forward to becoming one of your most reliable suppliers.
HY 80A Material grades and equivalents
Nimonic 80A /UNS N07080 / SEW VDIUV W. Nr. 2.4952 / AFNOR NC20TA
HY N80A Chemaical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
Mn |
Si |
P |
S |
Al |
Ti |
C |
Co |
B |
Zr |
Cu |
|
80A |
Min. |
Balance |
18 |
1.0 |
1.8 |
||||||||||
|
Max. |
21 |
3.0 |
1.0 |
1.0 |
0.02 |
0.015 |
1.8 |
2.7 |
0.1 |
2.0 |
0.008 |
0.15 |
0.2 |
HY N80A Physical properties:
|
Density |
8.19 g/cm3 |
|
Melting point |
1320-1365℃ |
HY N80 A minimum mechanical properties in the room temperature :
|
Status |
Tensile strength |
Yield strength |
Elongation |
|
HY N80A |
930 |
620 |
20 |
Characteristic as below:
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to 1500°F (815°C).
Used for gas-turbine components (blades, rings, and discs), bolts, tube supports in nuclear steam generators, die-casting inserts and cores, and exhaust valves in internal-combustion engines.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.