Our goal is to provide high quality products at competitive prices, and top-notch service to customers around the world. We are ISO9001, CE, and GS certified and strictly adhere to their quality specifications for Personlized Products Nickel Alloy Hastelloy B-2 UNS N10665 Supply to Surabaya, We are sincerely welcome good friends from numerous circles at dwelling and abroad come to cooperate!
HY B-2 Chemical compostion:
|
Alloy |
% |
Ni |
Mo |
Fe |
Cr |
Co |
C |
Mn |
V |
Si |
P |
S |
|
HY B-2 |
Min. |
Balance |
26 |
4 |
0.2 |
|||||||
|
Max. |
30 |
6 |
1 |
2.5 |
0.05 |
1 |
0.4 |
1 |
0.04 |
0.03 |
||
|
HY B-2-2 |
Min. |
Balance |
26 |
2 |
||||||||
|
Max. |
30 |
7 |
1 |
1 |
0.02 |
1 |
0.1 |
0.04 |
0.03 |
HY B-2 Physical properties:
|
Density |
9.24g/cm3 |
|
Melting point |
1330-1380℃ |
HY B-2 Alloy minimum mechanical properties in the room temperature:
|
Alloy state |
Tensile strength |
Yield strength |
Elongation |
|
HY B-2 |
690 |
310 |
40 |
Characteristic:
1. Control of iron and chromium content to a minimum to prevent the generation of β-phase Ni4Mo.
2. Excellent corrosion resistance of restore environment.
3. An excellent resist to concentration sulfuric acid medium and large number of non-oxidizing acid corrosion.
4. A very good resistance of chloride reduction of stress corrosion cracking (SCC).
5. Good corrosion resistance of various organic acids.
Metallurgical structure
HY B-2-2 is the face-centered cubic lattice structure. By controlling the content of iron and chromium at the minimum to reduce the processing brittle, prevent Ni4Mo precipitation during 700-870 ℃.
Corrosion resistance
Ni-Mo alloy HY B-2-2, the carbon and silicon content is extremely low, reducing the HAZ carbon and other impurities precipitation, so the weld has sufficient corrosion resistance. Alloy HY B-2-2 in the reduction of medium with very good corrosion resistance, such as a various temperature and concentration of hydrochloric acid. In the middle of the concentration of sulfuric acid solution (or contain a certain amount of chloride ions) also has very good corrosion resistance. At the same time can be used to acetic acid and phosphoric acid environment. Alloy material suitable only in the metallurgical structure and pure crystal structure in order to have the best corrosion resistance.
Applied field:
Alloy HY B-2-2 with a wide range of applications in the field of chemical, petrochemical, energy manufacturing and pollution control , particularly in the sulfuric acid, hydrochloric acid, phosphoric acid, acetic acid, and other industries.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
NEW 2016 Chrysler three hundred S Alloy Edition Sedan with a Gloss Black Paint finish. AWD that seats five with a three.two L V-six engine and an eight velocity computerized transmission. 19″ alluminum alloy rims with Michelin Primacy MXM4 tires. This sedan will come thoroughly loaded with keyless entry, distant get started, power locks, home windows, mirrors, Beats by Dre audio system, AM/FM, Sirius Sat radio, Lcd display screen in the entrance with back up digicam, leather all over with heated entrance and rear seats and so significantly a lot more. Come check out it out at Ponoka Chrysler and see what else it has to present, we are located on the south conclusion of Ponoka just off of HWY 2A.
Stock# 16C37644
Sarah Johnson,
Ponoka Chrysler
6510 39th Ave Ponoka, AB T4J 1J8
Toll Cost-free: 1(800) 265-6851
Cellphone: (403) 783-5383
Fax: (403) 783-8140
E-mail: sjohnson@ponokachrysler.com
Like us on Fb- https://www.facebook.com/PonokaChrysler/
Abide by us on Instargram- https://www.instagram.com/ponokadodge/
Abide by us on Twitter- https://twitter.com/PonokaDodgeRam
Abide by us on Pintrest- https://www.pinterest.com/ponokachrysler/