Professional High Quality Nickel Alloy Inconel 601 UNS N06601 in Florida

\

Short Introduction:


Product Detail

Product Tags

With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for Professional High Quality Nickel Alloy Inconel 601 UNS N06601 in Florida, We are sincerely welcome good friends from numerous circles at dwelling and abroad come to cooperate!


HY 601 Material grades and equivalents

Inconel 601 / GB NS313 / UNS N06601/W.Nr.2.4851 NiCr23Fe / AFNOR NC23FeA

HY 601 Chemaical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

Al

P

S

601

Min.

58

21

1.0

Max.

63

25

balance

0.1

1.5

0.5

1

1.7

0.02

0.015

HY 601 Physical properties

Density

8.1g/cm3

Melting point

1320-1370℃



HY 601 Alloy m inimum mechanical properties in the room temperature

Alloy state

Tensile strength
Rm N/mm2

Yield strength
R P0. 2N/mm2

Elongation
A 5 %

Brinell hardness
HB

Annealing treatment

650

300

30

-

Solution treatment

600

240

30

≤220

Characteristic as below:
1. Excellent inoxidability in the high temperature.
2. Good resistance to carbonizing.
3. Good inoxidabilitiy in sulfur atmosphere
4.Good mechanical property in both room temperature and high temperature.
5.Good resistance to stress corrosion cracking, 601 have high creep rupture strength since it limits the carbon content and grain size, so recommend to use for above 500℃ environment.

HY 601 Metallurgical structure:
601 is face-centered cubic lattice structure.

HY 601 Corrosion resistance
One of the mainly performance of 601 is inexorability in high temperature, even in very inclement conditions. If in the process of heating and cooling cycle, 601 can generate the dense layer of oxide film to get high spalling resistance. 601 have good carbonation resistance. With excellent inoxidability in the high temperature of sulfur atmosphere since it has high chromium and aluminum content.

HY 601 Application field:
1.The tray,basket and tool clamp in the heat treatment factory.
2.Steel shares at annealing and radiation control, high-speed gas burners, Industrial furnace silk screen.
3.Separate tank of ammonia reforming and catalytic support grid of nitric acid producing.
4.Exhaust system parts
5.Solid waste incinerator’s combustion chamber
6.Channel support and soot dealing parts.
7.Detoxification exhaust system components
8.Oxygen re-heater

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !