Cemented carbide YG20C/ ISO G40
YG20C Material grades and equivalents: ISO G40
Chemical composition(mass fraction)(%)
|
Alloy
|
WC |
TiC |
TaC (NbC) |
Co |
Other |
|
YG20C |
80 |
- |
20 |
Physical properties &minimum mechanical properties
|
Density/ g/cm |
Min Hardness/HRA |
Tensile strength/MPa |
Impact toughness j/cm |
Min Bending strength/ N/cm2 |
|
|
13.4-13.7 |
80 |
2200
|
7 |
2200
|
YG20C Characteristic as below:
High strength and good impact toughness.
YG20C Processing conditions and application:
It is suitable for the manufacture of cold heading, cold stamping and cold pressing dies for standard parts, bearings and tools, and the stamping die for the shell of the warhead. Used for cold heading dies and stamping dies, such as cold heading screws, nuts, cold punched steel balls, warheads, etc.
|
Regular shape for all kinds of alloys |
|||
|
Form |
Specification |
Supply Form |
Others |
|
Sheet |
Thickness:0.40-4.75mm,General Width:1000、1219、1500mm |
Whole Coil or piece of it |
Cold Annealed,Surface 2B、2E |
|
Plate |
Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) |
Whole Coil or piece of it |
Single hot rolling,Solid solution annealed state,Surface 1D |
|
Belt |
Thickness:0.10-3.0mm,Width:50-500mm |
Whole Coil or Specified size |
Cold Annealed,Surface 2B、2E |
|
Bar & Rod |
Rolled barΦ5-45mm,Length≤1500mm |
Polished Bar(circle、Square) |
Solution annealing,descaling |
|
Forged barΦ26-245mm,Length≤4000mm |
|||
|
Weld tube |
Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm |
Base on your requirement |
|
|
Seamless Tube |
Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm |
Base on your requirement |
|
|
Wire |
Outer diameterΦ0.1-13mm |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
|
Forged piece |
discs,rings,squares,blocks,slabs |
Base on your requirement |
Steel, Alloy |
|
Flangs |
All kinds of Flangs |
Base on your requirement |
Steel, Alloy |
|
Welding Material |
Coil wire Φ0.025mm-1.6mm |
Base on your requirement |
Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
|
Straight WireΦ1.6mm-4.0mm |
|||
|
Welding rodΦ1.2mm-4.0mm |
|||
|
Tube |
Elbow, three links, four links, different diameter size |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |
|
Explosive bonded laminate |
Raw Sheet Thickness≥2mm |
Base on your requirement |
Ni & Ni alloy, Ti & Ti alloy |